After 14 days of screed installation contractors can test the screed layer to ensure that it has developed appropriate compressive c and flexural f strength and is level enough to take on the final floor finish.
Compressive strength of floor screed.
Longfloor liquid cement screed works particularly well with underfloor heating systems.
The screed is then applied on top of existing concrete slabs as a finishing layer for indoor floors or as a means of levelling off the floor.
A floor screed is usually a cementitious material made from a 1 3 or 1 4 5 ratio of cement to sharp sand.
24 6 n mm flexural strength bs 6319 3.
The concrete on which the screed or topping is to be laid should be hard and strong i e.
81 n mm tensile strength bs 6319 7.
The strength of the precast is generally between 40 and 60n mm and the structural topping is 25 30n mm.
It can be supplied as a c20 or c25mm n2 compressive strength product.
Versatile applicable in 8 200 mm thickness for both interior and exterior time saving directly coatable with resinous coatings after 2 48 hours without preparation screed with very high mechanical strength compressive strength of 60 n mm2 en 13813.
Approvals and certificates determination of compressive strength astm c579.
Sand cement screed subfloors with polymer additives that achieve a compressive strength of 20 mpa and tensile strength of 1 5 mpa are considered acceptable.
The standard states that a screed produced with these material proportions would meet the expected criteria for in situ crushing resistance.
There are many proprietary screeds on the market and information about these can be obtained from the manufacturer.
Resistant screed for areas with extreme wear and tear.
It is also stated that a screed with a compressive strength class of c20 or c25 would also meet the in situ crushing requirements.
Characteristic strength of at least 20 mpa.
Traditional screed is mostly a mixture of sand and cement mixtures that are blended on site and applied.
Weak friable concrete is not suitable as a base for a screed or topping as the achievement of adhesion between such material and the screed or topping is not possible.
What are the issues.
The finishing cover of laminate carpet tile stone etc.
Compressive strength may be expected of 35 n mm2 or higher 20 c.
Is then able to be applied on top.
Suitable on approved primers on concrete substrates.
Can be used as mid coat or finish coat.